Green shrinkage seen in

A
Phosphate bonded investment.
B
Ethyl silicate bonded investment.
C
Gypsum bonded investment.
D
All of the above.
High-Yield Explanation
• Green shrinkage: -Occurs during heating of silicate investments. -Occurs due to loss of alcohol & water during phase(168ºC) to form a concentrated, hard gel. This also leads to volumetric contraction of the mould