Dental General 914d71a5 The strength attained by amalgam within 24 hours is: A More than 60% B More than 70% C More than 80% D More than 90% High-Yield Explanation The strength attained by amalgam within 24 hours is more than 90%. Reference: Marzouk Operative dentistry, pg-111