Full 2L QBank
Dental General 0a4cc8d8

ZOE is not used for permanent cementation because of?

A
Less strength
B
High solubility
C
Poor marginal seal
D
Poor pulpal protection
High-Yield Explanation
DISADVANTAGES It does not adhere well to enamel and dentin; hence, it causes microleakage and cannot be used for interim and long-term restorations. Due to its low strength and high solubility, it cannot be used for permanent cementation(1st choice will be low strength then low solubility if asked in exams). Its solubility is highest among all cements. Ref: Materials used in dentistry, S. Mahalaxmi pg 267